Wadah Molibdenum
-
Laris Rega Paling Apik 99,95% Kemurnian Minimal Wadhah Molibdenum / Pot Kanggo Leleh
Kemurnian: 99,97% Mo
Suhu kerja: 1300-1400Centigrade: Mo1
2000 Celcius: TZM
1700-1900Centigrade: MLa
Wektu pangiriman: 10-15 dina
Bahan liyane: TZM, MHC, MO-W, MO-RE, MO-LA, Mo1
Dimensi & Kubus: Miturut kabutuhan utawa gambar sampeyan
Lumahing: Rampungake puteran, Grinding