Parameter produk
Merk | HSG |
Standar | ASTMB760-07;GB/T3875-83 |
sasmita | W1, W2, WAL1, WAL2 |
Kapadhetan | 19,2 g/cc |
Kemurnian | ≥99,95% |
Ukuran | Ketebalan 0.05mm min * Jembar maksimal 300mm * L 1000mm maksimal |
lumahing | Black/Alkali cleaning/polesan |
Titik lebur | 3260C |
Proses | rolling panas |
komposisi kimia
Komposisi kimia | ||||||||||
Isi pengotor (%), ≤ | ||||||||||
Al | Ca | Fe | Mg | Mo | Ni | Si | C | N | O | |
imbangan | 0.002 | 0.005 | 0.005 | 0.003 | 0.01 | 0.003 | 0.005 | 0.008 | 0.003 | 0.005 |
Ukuran lan variasi sing diidini
kekandelan | Toleransi Kekandelan | Jembar | Toleransi Jembar | dawa | Toleransi dawa | |
I | II | |||||
0.10-0.20 | ± 0,02 | ± 0,03 | 30-150 | ±3 | 50-400 | ±3 |
> 0.20-0.30 | ± 0,03 | ± 0,04 | 50-200 | ±3 | 50-400 | ±3 |
> 0.30-0.40 | ± 0,04 | ± 0,05 | 50-200 | ±3 | 50-400 | ±3 |
> 0.40-0.60 | ± 0,05 | ± 0,06 | 50-200 | ±4 | 50-400 | ±4 |
> 0,60-0,80 | ± 0,07 | ± 0,08 | 50-200 | ±4 | 50-400 | ±4 |
> 0.8-1.0 | ± 0,08 | ± 0,10 | 50-200 | ±4 | 50-400 | ±4 |
> 1.0-2.0 | ± 0,12 | ± 0,20 | 50-200 | ±5 | 50-400 | ±5 |
> 2.0-3.0 | ± 0,02 | ± 0.30 | 50-200 | ±5 | 50-400 | ±5 |
> 3.0-4.0 | ± 0,03 | ± 0,40 | 50-200 | ±5 | 50-400 | ±5 |
> 4.0-6.0 | ± 0,04 | ± 0,50 | 50-150 | ±5 | 50-400 | ±5 |
Fitur
Titik leleh dhuwur, Kapadhetan dhuwur, tahan oksidasi suhu dhuwur, umur dawa, tahan korosi.
Tungsten tabung digunakake digunakake ing tabung pangayoman thermocouple, tungku kristal sapir lan tungku suhu dhuwur, etc. Bango bisa nyedhiyani tabung tungsten kanthi tliti dhuwur, lumahing Rampung, ukuran sakcara, lan deformasi suhu dhuwur.
Aplikasi
Aplikasi Plat Tungsten: Plat tungsten kemurnian A99.95%.
1. Komponen tahan panas: tameng panas, unsur panas saka tungku vakum suhu dhuwur.
2. Tungsten sputtering target kanggo nutupi vakum lan nutupi penguapan.
3. Komponen elektronik lan semi-conduct.
4. Ion implanted komponen.
5. Perahu tungsten kanggo tungku kristal sapir lan tungku vakum.